Results of nanoindentation, XRD and microscopic studies of bacterial cellulose

收藏
Most Wiedzy Open Research Data Catalog2026-04-17 收录
下载链接:
https://mostwiedzy.pl/en/open-research-data/results-of-nanoindentation-xrd-and-microscopic-studies-of-bacterial-cellulose,12270921211221516-0
下载链接
链接失效反馈
官方服务:
资源简介:
The archive contains the results of research on BNC bacterial biocellulose, which was modified in two ways. When BNC was synthesized, it was subjected to in situ modification involving the addition of hyuloronic acid to the bacterial medium. The second way of ex situ modification consisted of soaking the BNC in water and then convectionally drying it at 25 C and 105 C and also freeze-drying it. XRD, nanoindentation and also Raman spectra were performed, and pore distribution and size were determined. The relationship between the structure of modified and unmodified BNC and its mechanical properties was demonstrated. The studies were performed in the context of BNC applications for cardiovascular implants.
提供机构:
Alicja Stanisławska
二维码
社区交流群
二维码
科研交流群
商业服务