Rocking scans of Pd/Al$_2$O$_3$ under CH$_4$ oxidation conditions - Cycle II
收藏DataCite Commons2025-08-15 更新2026-04-25 收录
下载链接:
https://bib-pubdb1.desy.de/record/636456
下载链接
链接失效反馈官方服务:
资源简介:
Movies of the HEGIXRD rocking scans of Pd/Al$_2$O$_3$ catalyst for full CH$_4$ oxidation under operation during the second experiment cycle. The scans are recorded at 523K, 573K, 623K, 673K, and 723K with a reactor pressure of 100mbar, a total flow 100ml/min and a composition of 20% O2, 0.1% CH4, and 79.9% Ar.
提供机构:
Deutsches Elektronen-Synchrotron, DESY, Hamburg
创建时间:
2025-08-15