遇见数据集

Small punch creep test data for AISI 316L ar material at 700 °C and a load of 500 N (specimen identifier CK-047-700C-500N)

收藏
DataCite Commons2023-08-30 更新2025-04-16 收录
官方服务:

资源简介:

Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Several test materials have been tested. For estimating the tensile properties a series of tests were carried out at room and elevated temperatures. Further tests were performed at varying temperatures between 77K and room temperature to determine the ductile to brittle transition temperature (DBTT). Creep tests have also been carried out.

创建时间:
2018-04-25