High resolution crystallographic and chemical characterisation of iodine induced stress corrosion crack tips formed in irradiated and non-irradiated zirconium alloys - Supporting data

收藏
Zenodo2020-07-29 更新2026-05-25 收录
数据链接:
官方服务:

资源简介:

Data related to High resolution crystallographic and chemical characterisation of iodine induced stress corrosion crack tips formed in irradiated and non-irradiated zirconium alloys: Conor Gillen, Alistair Garner, Pia Tejland, Philipp Frankel,<br> High resolution crystallographic and chemical characterisation of iodine induced stress corrosion crack tips formed in irradiated and non-irradiated zirconium alloys, Journal of Nuclear Materials, Volume 519, 2019, Pages 166-172, ISSN 0022-3115,<br> https://doi.org/10.1016/j.jnucmat.2019.03.027. Datafiles for STEM-EDX analysis - STEM-EDX.zip Datafiles for TKD analysis - TKD.zip Datafiles for NanoSIMS analysis - 1: NanoSIMS raw data file (.im file) with all 160 planes and data for all ion signals acquired. Can be opened with the OpenMIMS plugin for ImageJ or other NanoSIMS software. 2: NanoSIMS processed data file (.nrrd file) which is drift corrected and can be opened with the OpenMIMS plugin for ImageJ

提供机构:
Zenodo
创建时间:
2019-04-09
二维码
社区交流群
二维码
科研交流群
商业服务