Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.004 mN (thirty-third nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新90
Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.004 mN (twenty-second nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新50
Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.002 mN (thirty-second nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新40
Nanoindentation (single cycle) test data for Model Alloy (Fe) material at 23 °C and maximum indenter force of 50.022 mN
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新60
Nanoindentation (single cycle) test data for Model Alloy (Fe) material at 23 °C and maximum indenter force of 100.02 mN (first nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新40