OSU: Destructive Test, Aluminum Specimen, Water Depth = 257.2 cm
收藏数据链接:
官方服务:
资源简介:
In this experiment, the load cell will be positioned to make contact with the centroid of the broad face of the aluminum shipping container specimen. The idea is to start off at the slowest velocities, and then jump to the highest in order to see if we can damage the specimen. DOI Title: In-Water Destructive Test, Water Depth = 257.2 cm: Measurements of free surface variation, impact force.