Uniaxial creep test data for 14 MoV 6 3 material at 600 °C and a stress of 77.2 MPa
收藏官方服务:
资源简介:
A collection of elastic modulus and long-time creep fracture data for 1/2 CrMoV steel.
创建时间:
2015-11-23

A collection of elastic modulus and long-time creep fracture data for 1/2 CrMoV steel.