遇见数据集

Differential scanning calorimetry measurements of samples of commercial polycaprolactone

收藏
Zenodo2025-10-08 更新2026-05-26 收录
官方服务:

资源简介:

Differential Scanning Calorimetry (standard) and Modulated Differential Scanning Calorimetry (MDSC) measurements of polycaprolactone (PCL) samples. The samples were measured in Centro de Investigación, Tecnología e Innovación (CITIUS) at University of Seville, Spain. The used polymer is PCL-600 C and it was produced by eSUN. There are two file formats: txt and 001, which can be opened by the TA Instruments’ Universal Analysis program. The files are labelled as follows: PCL_method The following protocol was used to produce the data: DSC:-Ramp 10.00 °C/min to 150.00 °C -Equilibrate at -80.00 °C -Ramp 10.00 °C/min to 150.00 °C MDSC:-Ramp 10.00 °C/min to 150.00 °C -Equilibrate at -80.00 °C -Modulate ± 1.00 °C every 60 s -Isothermal for 5.00 min -Ramp 2.00 °C/min to 150.00 °C

提供机构:
Zenodo
创建时间:
2025-10-08
二维码
社区交流群
二维码
科研交流群
商业服务