Results obtained through Differential Scanning Calorimetry (DSC) for silica, lipase enzyme, immobilized lipase, produced lipase, immobilized produced lipase.
收藏NIAID Data Ecosystem2026-05-02 收录
数据链接:
官方服务:
资源简介:
Results obtained through Differential Scanning Calorimetry (DSC) for silica, lipase enzyme, immobilized lipase, produced lipase, immobilized produced lipase.
创建时间:
2025-05-07