Comparison of residual stresses in TC4 specimens after LSP with different parameters:(a) overlapping rate 0%; (b) overlapping rate 25%; (c) overlapping rate 50%
收藏官方服务:
资源简介:
TC4 specimen thickness δ= 7 mm, with an error of ± 0.1mm. Test the non LSP specimens and the LSP8, LSP10, and LSP12 specimens subjected to impact strengthening at laser power densities of 8 GW/cm2, 10 GW/cm2, and 12 GW/cm2, respectively. Residual stress test results
提供机构:
Science Data Bank创建时间: