Nanoindentation (single cycle) test data for Fused silica ar material at 23.8 °C and maximum indenter force of 10.018 mN (sixth nominally repeat test)

收藏
DataCite Commons2020-10-05 更新2025-04-16 收录
官方服务:

资源简介:

Data created at NPL, United Kindom during the CEN Workshop NATEDA on nanoindentation test data, itself a component of the H2020 M4F project funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.