Data for "Mechanical characterization and strain-rate sensitivity measurement of Ti-7333 alloy based on nanoindentation and crystal plasticity modeling"

收藏
Mendeley Data2024-01-31 更新2024-06-26 收录
下载链接:
https://data.mendeley.com/datasets/ddxtvjjfdk
下载链接
链接失效反馈
官方服务:
资源简介:
the supporting data for paper entitled 'Mechanical characterization and strain-rate sensitivity measurement by nanoindentation and crystal plasticity finite element modeling: Application to Ti-7Mo-3Nb-3Cr-3Al near β titanium alloy'