Effect of heat treatment on the high-temperature wear resistance and oxidation behavior of laser powder bed fusion-manufactured Inconel 718 alloy
收藏Mendeley Data2026-09-08 收录
官方服务:
资源简介:
The HT specimens demonstrated better wear resistance than the as-built LPBF specimen, as evidenced by a reduction in the average coefficient of friction from 0.74 to 0.69 after heat treatment.
经热处理(Heat Treatment, HT)的试样展现出优于原始成形激光粉末床熔融(Laser Powder Bed Fusion, LPBF)试样的耐磨性能,该性能优势可通过热处理后平均摩擦系数从0.74降至0.69得以验证。