Data created at the NCBJ, Poland during the H2020 project on multiscale modeling for fusion and fission materials. The research leading to these results has been carried out in the frame of EERA Joint Program for Nuclear Materials and is funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.