资源简介:

Figure Captions Fig. 1. SEM images of various coatings: (a) UMAO, (b) UMAO/CS, (c) UMAO/CS/IC(10V3 M), (d) UMAO/CS/IC(20V3M) and (e) UMAO/CS/IC(20V5M). Fig. 2. SEM cross-section morphologies of various coatings: (a) UMAO, (b) UMAO/CS, (c) UMAO/CS/IC(10V3M), (d) UMAO/CS/IC(20V3M) and (e) UMAO/CS/IC(20V5M). Fig. 3. (a) X-ray diffraction patterns and (b) FT-IR spectra of various coatings. Fig. 4. (a) AFM images and (b) digital photographs of water droplets of various coatings. Fig. 5. (a) Potentiodynamic polarization curves, (b) Nyquist plots, and (c) Bode plots of various samples. The symbols are the experimental data and the solid lines are fitting data. Fig. 7. SEM images of cells cultured on various coatings: (a) UMAO, (b) UMAO/CS, and (c) UMAO/CS/IC. Fig. 8. CLSM images of cells cultured for 0.5 h on various coatings: (a) UMAO, (b) UMAO/CS, and (c) UMAO/CS/IC. Fig. 9. Adhesion of MC3T3-E1 cells cultured on various coatings for 0.5, 1, 2, and 6 hours. Data are presented as the mean ± SD, n = 4, (#) p < 0.05 and (##) p < 0.01 compared with those of UMAO, (*) p < 0.05 and (**) p < 0.01 compared with those of UMAO/CS. Fig. 10. Proliferation of MC3T3-E1 cells cultured on various coatings for 1, 3, and 5 days. Data are presented as the mean ± SD, n = 4, (#) p < 0.05 and (##) p < 0.01 compared with those of UMAO, (*) p < 0.05 and (**) p < 0.01 compared with those of UMAO/CS.

图注 图1 各类涂层的扫描电子显微镜(Scanning Electron Microscope, SEM)图像:(a) UMAO,(b) UMAO/CS,(c) UMAO/CS/IC(10V3 M),(d) UMAO/CS/IC(20V3 M) 及 (e) UMAO/CS/IC(20V5 M)。 图2 各类涂层的扫描电子显微镜截面形貌:(a) UMAO,(b) UMAO/CS,(c) UMAO/CS/IC(10V3 M),(d) UMAO/CS/IC(20V3 M) 及 (e) UMAO/CS/IC(20V5 M)。 图3 (a) 各类涂层的X射线衍射(X-ray Diffraction, XRD)图谱,(b) 傅里叶变换红外(Fourier Transform Infrared, FT-IR)光谱。 图4 (a) 各类涂层的原子力显微镜(Atomic Force Microscope, AFM)图像,(b) 各类涂层的水滴数码照片。 图5 (a) 动电位极化曲线,(b) 奈奎斯特(Nyquist)图,以及(c) 博德(Bode)图。图中符号为实验实测数据,实线为拟合所得数据。 图7 各类涂层表面培养细胞的扫描电子显微镜图像:(a) UMAO,(b) UMAO/CS,(c) UMAO/CS/IC。 图8 各类涂层表面培养0.5小时的细胞的共聚焦激光扫描显微镜(Confocal Laser Scanning Microscope, CLSM)图像:(a) UMAO,(b) UMAO/CS,(c) UMAO/CS/IC。 图9 MC3T3-E1细胞在各类涂层上分别培养0.5、1、2及6小时后的黏附情况。数据以平均值±标准差表示,每组样本量n=4;与UMAO组相比,(#) p<0.05、(##) p<0.01;与UMAO/CS组相比,(*) p<0.05、(**) p<0.01。 图10 MC3T3-E1细胞在各类涂层上分别培养1、3及5天后的增殖情况。数据以平均值±标准差表示,每组样本量n=4;与UMAO组相比,(#) p<0.05、(##) p<0.01;与UMAO/CS组相比,(*) p<0.05、(**) p<0.01。

创建时间:
2019-01-30
二维码
社区交流群
二维码
科研交流群
商业服务