Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.001 mN (tenth nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新80
Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.003 mN
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新60
Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 10.007 mN (sixth nominally repeat test)
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 un
DataCite Commons2020-10-05 更新90
Uniaxial tensile test data for AISI 316 L(N) IG material at 288 °C (first nominally repeat test)
Data created at the JRC during the Horizon 2020 MEACTOS project on mitigating environmentally assisted cracking through optimization of surface condition. This project has received funding from the Eu
DataCite Commons2022-03-18 更新70