Data for: Evolution behavior of liquid film in the heat-affected zone of laser cladding non-weldable nickel-based superalloy
收藏Mendeley Data2026-04-18 收录
下载链接:
https://data.mendeley.com/datasets/b9trv5djj5
下载链接
链接失效反馈官方服务:
资源简介:
Phase composition in K447A superalloy obtained via EPMA and the friction of solid in the grain boundary of K447A superalloy obtained via JMatPro software are listed.