Differential Scanning Calorimetry of Native Silk Feedstock Dataset
收藏数据链接:
官方服务:
资源简介:
Origin Project File containing all the data used for creation of main figures and supplementary figures in the publication "Differential Scanning Calorimetry of Native Silk Feedstock"https://doi.org/10.1002/mabi.201800228 <br>
创建时间:
2018-05-31