Data for: Effect of Temperature on Electrochemical Pitting Corrosion Behavior of 316L Stainless Steel in MDEA Solution Containing Chloride

收藏
NIAID Data Ecosystem2026-03-12 收录
官方服务:

资源简介:

(1) Potentiodynamic polarization data of 316L SS in two solution at different temperatures: (a) plain MDEA solution (b) MDEA solution containing 1.0 wt % Cl−. (2)Breakdown potenital- temperature data for 316L SS in MDEA solution containing 1.0 wt % Cl−. (3)Potentiostatic polarization data of 316L SS at an anodic potential of 300 mV vs. Ag/AgCl (0.1 mol/L-1 KCl) in two solution at different temperatures and elapsed time: (a) plain MDEA solution (b) MDEA solution containing 1.0 wt % Cl−. (4)Data for EIS plots of the corrosion of 316L SS in plain MDEA amine solution at different temperatures: (a) Nyquist plot (b) impedance amplitude (c) phase angle. (5) Data for EIS plots of the corrosion of 316L SS in MDEA amine solution containing 1.0 wt% Cl− at different temperatures: (a) Nyquist plot (b) impedance amplitude (c) phase angle.

创建时间:
2020-11-21
二维码
社区交流群
二维码
科研交流群
商业服务