CEN/WS NATEDA nanoindentation test data
收藏DataCite Commons2024-02-08 更新2024-07-13 收录
下载链接:
https://odin.jrc.ec.europa.eu/alcor/DOICatalogDisplay.html?p_DOI5=51
下载链接
链接失效反馈官方服务:
资源简介:
JRC and NPL nanoindentation test data created during the inter-laboratory data exchange case study of the CEN Workshop NATEDA, itself a component of the H2020 M4F project funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.