High Temperature Micromechanics Ni-based Superalloys: Creep, Stress Relaxatio...
收藏B2FIND2026-04-25 收录
官方服务:
资源简介:
In this study, in-situ high-temperature loading investigations will be performed to characterise the micromechanics of a high strength alloy 720Li, during stress relaxation in...