Experimental Dataset for Friction Stir Processing, Electrochemical Corrosion, and Stress Corrosion Cracking of ZE41 and AZ91D Magnesium Alloys
收藏资源简介:
This dataset encompasses experimental data related to friction stir processing (FSP), electrochemical corrosion and sustained-load stress corrosion cracking of ZE41 and AZ91D magnesium alloys. Sensor Core Dataset The core data set consists of 14 records of SCC time-series measurements with corresponding system time, elapsed time and load evolution (indicated load for exposure to 3.5 wt. at nominal loading levels (20-100% of yield strength) in a 5 M % NaCl solution. The measured SCC records are: AZ91D base metal, AZ91D friction stir processed conditions at 20, 40, 60 and 80% YS (in that order of decreasing active SCC rate) together with ZE41 friction stir processed conditions at 20, 40, 60 and 80% YS. The repo also includes collection of standardised csv files, data dictionary, record inventory, quality-control notes, raw-versus-reported cross-checks for five-level friction stir processing parameter tables (e.g. Central Composite Design matrices bluever 20 runs ZE41 and AZ91D per sign level; Tables S3-S4), and potentiodynamic polarization summary data from the base metal directly adjacent to TMAZ and stir-zone condition (Table S5). 100% YS from synthetic reconstructions of ZE41-BM and ZE41-FSP are not shown in the main experimental dataset.
本数据集涵盖了ZE41与AZ91D镁合金的搅拌摩擦加工(Friction Stir Processing, FSP)、电化学腐蚀及持续载荷应力腐蚀开裂(Stress Corrosion Cracking, SCC)相关的实验数据。传感器核心数据集:核心数据集包含14组应力腐蚀开裂时序测量记录,配套记录了系统时间、流逝时长与载荷演化数据;实验于3.5 wt.%氯化钠溶液中开展,载荷设置为标称载荷水平(屈服强度的20%~100%),载荷值对应暴露工况的指示载荷。所测得的应力腐蚀开裂记录依次为:AZ91D母材、分别在20%、40%、60%、80%屈服强度载荷下的AZ91D搅拌摩擦加工态(该顺序对应应力腐蚀开裂活性速率递减),以及分别在20%、40%、60%、80%屈服强度载荷下的ZE41搅拌摩擦加工态。本数据集仓库还包含标准化逗号分隔值(CSV)文件集、数据字典、记录清单、质量控制说明、原始数据与报告数据交叉校验文件,以及针对五级搅拌摩擦加工参数表(例如中心复合设计矩阵,每个符号水平下为ZE41和AZ91D各设置20组试验;表S3~S4)的相关校验项,此外还包含紧邻热机械影响区(Thermo-Mechanically Affected Zone, TMAZ)与搅拌区的母材的动电位极化汇总数据(表S5)。基于ZE41母材(ZE41-BM)和ZE41搅拌摩擦加工态(ZE41-FSP)的100%屈服强度合成重构数据未纳入主实验数据集。