Data for: Helium-ion microscopy, helium-ion irradiation and nanoindentation of Eurofer 97 and ODS Eurofer

收藏
Mendeley Data2026-04-18 收录
下载链接:
https://data.mendeley.com/datasets/wk5639d3xy
下载链接
链接失效反馈
官方服务:
资源简介:
A set of He-ion irradiations was aimed at visualizing irradiation-induced changes directly in the HIM using the video mode. Video files for Eurofer 97 and ODS Eurofer of the in-situ irradiation experiments in the HIM (Ion energy 30 keV, maximum fluence 2E18 He ions/cm2, linear time scale) are provided. We have observed that the onset of blistering takes place slightly above a fluence of 5E17 He ions/cm2 for Eurofer 97 and slightly below this value for ODS Eurofer. For more details read the main text.

本数据集包含一组氦离子辐照实验,旨在通过视频模式直接借助氦离子显微镜(Helium Ion Microscope, HIM)观测辐照诱导的微观结构变化。本次提供了Eurofer 97与氧化物弥散强化Eurofer 97(Oxide Dispersion Strengthened Eurofer, ODS Eurofer)在氦离子显微镜内开展的原位辐照实验的视频文件,实验参数如下:离子能量30 keV,最大注量2×10¹⁸ 氦离子/平方厘米,时间尺度为线性刻度。经观测发现,Eurofer 97的起泡起始注量略高于5×10¹⁷ 氦离子/平方厘米,而ODS Eurofer的起泡起始注量略低于该数值。更多实验细节请参阅正文。
创建时间:
2017-08-06
二维码
社区交流群
二维码
科研交流群
商业服务