资源简介:

This dataset was used to predict the occurrence of ethanol-based pitting corrosion in AA1050 using binary classification. It consists of five system descriptors: Temperature (°C) Chloride content (ppm) Water content (ppm) Grit size of polishing paper Ethanol content (% by volume) of the fuel The target variable, named "corr," indicates corrosion occurrence, where 1 means corrosion occurred and 0 means no corrosion occurred. The dataset comprises 115 samples in total: 105 samples where corrosion occurred and 10 samples where no corrosion occurred.

本数据集旨在通过二分类任务预测AA1050铝合金的乙醇基点蚀发生情况。该数据集包含5项系统输入特征: 1. 温度(℃) 2. 氯化物含量(ppm) 3. 水分含量(ppm) 4. 抛光砂纸粒度 5. 燃料中乙醇的体积分数(%) 目标变量命名为"corr",用于表征腐蚀发生状态:取值为1时代表发生腐蚀,取值为0时代表未发生腐蚀。本数据集总计包含115个样本,其中发生腐蚀的样本共105个,未发生腐蚀的样本共10个。