Strain accumulation and fatigue crack initiation at pores and carbides in a SX superalloy at room temperature: x-ray computed tomography, tabulated data and modelling datasets
收藏DataCite Commons2020-09-20 更新2025-04-17 收录
下载链接:
https://eprints.soton.ac.uk/id/eprint/419493
下载链接
链接失效反馈官方服务:
资源简介:
This dataset includes the data presented in the journal paper Strain accumulation and fatigue crack initiation at pores and carbides in a SX superalloy at room temperature.
提供机构:
University of Southampton
创建时间: