In-situ neutron diffraction study of TWIP in a Ni based superalloy

收藏
DataCite Commons2020-12-01 更新2025-04-16 收录
下载链接:
https://data.isis.stfc.ac.uk/doi/STUDY/113049316/
下载链接
链接失效反馈
官方服务:
资源简介:
Twinning induced plasticity (TWIP) has been studied extensively regarding low stacking fault energy (SFE) materials such as steels where the specific deformation mechanism enhances both strength and ductility. In Ni-based alloys, activation of twinning is difficult due to their high SFE. Our recent work revealed that outstanding mechanical properties can be obtained in a Ni-based superalloy by inducing the TWIP effect at a low deformation temperature. Ab initio calculations indicates that SFE is not the controlling effect. To investigate the underlying mechanisms further an in-situ neutron diffraction investigation is proposed. Lattice strain changes and grain rotations with deformation at RT and 77 K derived from the experiment will be correlated to microstructural studies by laboratory techniques to explore the mechanisms and conditions for activating TWIP in high SFE alloys.
提供机构:
ISIS Facility
创建时间:
2020-12-01
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作