Effect of annealing twins, strain-recrystallization processing and δ-phase fraction on microtexture and evaluation of mechanical properties of nickel-based superalloy 718

收藏
NIAID Data Ecosystem2026-05-01 收录
官方服务:

资源简介:

EBSD Maps for the work "Effect of annealing twins, strain-recrystallization processing and δ-phase fraction on microtexture and evaluation of mechanical properties of nickel-based superalloy 718"