The downloadable results were the output HR-EBSD analysis for Samples 1, 2 & 3. The zip file includes data for GND density maps, stress tensor component maps, and rotation tensor component maps. Note, that all maps are given in the sample reference frame. The individual files are given in a '.mat' filetype which can be opening with Matlab. Further details of the experimental configuration are given in the manuscript for this work.

可下载的结果为样品1、2与3的高分辨率电子背散射衍射(HR-EBSD)分析输出产物。该压缩包包含几何必需位错(Geometrically Necessary Dislocations, GND)密度分布图、应力张量分量分布图以及旋转张量分量分布图的相关数据。请注意,所有分布图均以样品参考系为基准进行构建。单个数据文件均采用.mat文件格式,可通过Matlab软件打开。本研究的实验配置详细信息已在本文手稿中完整呈现。