Brunauer-Emmett-Teller (BET) surface analysis of titanium dioxide (TiO2) and silicon dioxide (SiO2) used for coating of expanded polystyrene spheres (EPS)
收藏Most Wiedzy Open Research Data Catalog2026-04-17 收录
数据链接:
官方服务:
资源简介:
Data refer to the results of BET surface area of TiO2 and SiO2 powders used for coating of expanded polystyrene spheres. The detailed measurement and equipment data was described in readme BET.txt file.TiO2 was treated firstly in autoclave at 150 C degrees for 1h, then was further heat treated in Ar at 400 C degrees. As a raw material TiO2 was used, which was a semiproduct from the industrial production of titania white by sulphur method. The raw material was mostly amorphous and contained some nuclei of rutile and sulphur species. SiO2 was obtained via modified Strober method.