Data for: Effect of Temperature on Electrochemical Pitting Corrosion Behavior of 316L Stainless Steel in MDEA Solution Containing Chloride
收藏资源简介:
(1) Potentiodynamic polarization data of 316L SS in two solution at different temperatures: (a) plain MDEA solution (b) MDEA solution containing 1.0 wt % Cl−. (2)Breakdown potenital- temperature data for 316L SS in MDEA solution containing 1.0 wt % Cl−. (3)Potentiostatic polarization data of 316L SS at an anodic potential of 300 mV vs. Ag/AgCl (0.1 mol/L-1 KCl) in two solution at different temperatures and elapsed time: (a) plain MDEA solution (b) MDEA solution containing 1.0 wt % Cl−. (4)Data for EIS plots of the corrosion of 316L SS in plain MDEA amine solution at different temperatures: (a) Nyquist plot (b) impedance amplitude (c) phase angle. (5) Data for EIS plots of the corrosion of 316L SS in MDEA amine solution containing 1.0 wt% Cl− at different temperatures: (a) Nyquist plot (b) impedance amplitude (c) phase angle.
(1) 动电位极化(Potentiodynamic polarization)数据:316L不锈钢(316L SS)在两种不同温度的溶液中的动电位极化测试数据,分为(a) 空白甲基二乙醇胺(MDEA)溶液,(b) 含1.0 wt%氯离子(Cl−)的MDEA溶液。 (2) 316L不锈钢在含1.0 wt% Cl−的MDEA溶液中的击穿电位-温度关系数据。 (3) 恒电位极化(Potentiostatic polarization)数据:316L不锈钢在相对于以0.1 mol·L⁻¹ KCl为电解质的Ag/AgCl参比电极的300 mV阳极电位下,于两种溶液中、不同温度及不同时长下的恒电位极化测试数据,分为(a) 空白MDEA溶液,(b) 含1.0 wt% Cl−的MDEA溶液。 (4) 电化学阻抗谱(EIS, Electrochemical Impedance Spectroscopy)测试数据:316L不锈钢在空白MDEA胺溶液中、不同温度下的腐蚀电化学阻抗谱数据,分为(a) 奈奎斯特(Nyquist)图,(b) 阻抗模值,(c) 相位角。 (5) 316L不锈钢在含1.0 wt% Cl−的MDEA胺溶液中、不同温度下的腐蚀电化学阻抗谱数据,分为(a) 奈奎斯特图,(b) 阻抗模值,(c) 相位角。