Nanoindentation (single cycle) test data for Fused silica ar material at 23 °C and maximum indenter force of 10.032 mN
收藏官方服务:
资源简介:
Data created at the European Commission JRC during the CEN Workshop NATEDA on nanoindentation test data, itself a component of the H2020 M4F project funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.
本数据集由欧洲委员会联合研究中心(Joint Research Centre, JRC)在欧洲标准化委员会(Comité Européen de Normalisation, CEN)举办的NATEDA纳米压痕测试数据专题研讨会期间编制完成,其作为H2020(Horizon 2020)框架计划下M4F项目的组成部分,由2014-2018年欧洲原子能共同体(Euratom)研究与培训计划通过编号为755039的资助协议提供资助。
创建时间:
2020-04-24