Data for: Electrochemical characteristic and stress corrosion behavior of API X70 high-strength pipeline steel under a simulated disbonded coating in an artificial seawater environment
收藏NIAID Data Ecosystem2026-03-11 收录
官方服务:
资源简介:
Data for: Electrochemical characteristic and stress corrosion behavior of API X70 high-strength pipeline steel under a simulated disbonded coating in an artificial seawater environment
创建时间:
2019-05-30