Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 2.003 mN (seventy-fifth nominally repeat test)
收藏官方服务:
资源简介:
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.
本数据集由欧盟委员会联合研究中心(European Commission Joint Research Centre, JRC)在面向聚变与裂变材料的多尺度建模H2020项目M4F(Multiscale Modeling for Fusion and Fission Materials)期间构建。该项目由2014-2018年欧洲原子能共同体(Euratom)研究与培训计划资助,资助协议编号为755039。
创建时间:
2020-01-14