Data for "The effect of phase chemistry on the extent of strengthening mechanisms in model Ni-Cr-Al-Ti-Mo based superalloys"
收藏DataCite Commons2024-12-17 更新2024-08-25 收录
下载链接:
https://www.repository.cam.ac.uk/handle/1810/275820
下载链接
链接失效反馈官方服务:
资源简介:
* Composition data of the gamma and gamma prime phases obtained using STEM-EDX. * Proximity histogram composition data across a gamma-gamma prime interface obtained using 3DAPT. * Bulk alloy compositions obtained using SEM-EDX. * Load vs extension data obtained during compression testing of the alloys. * Neutron diffraction patterns in the form of intensity vs 2theta data for each of the alloys. * Particle sizes for the gamma prime precipitates obtained from image analysis of the micrographs obtained by electron microscopy. These data are unsorted.
* 利用扫描透射电子显微镜-能量色散X射线能谱(STEM-EDX)测得的γ相(gamma)与γ’相(gamma prime)成分数据。
* 利用三维原子探针层析技术(3DAPT)测得的γ-γ’界面附近成分邻近直方图数据。
* 利用扫描电子显微镜-能量色散X射线能谱(SEM-EDX)测得的块体合金成分数据。
* 该类合金压缩试验过程中获取的载荷-延伸量数据。
* 各合金以强度-2θ为变量的中子衍射图谱数据。
* 通过电子显微镜采集的显微图像经图像分析得到的γ’相析出颗粒尺寸数据,该批数据未经过排序处理。