Initial experiments with Uroprint tensile tester V1-1
收藏资源简介:
Data for tensile tests on PLMA samples as measured on the version 1 tensile tester. Data is contained within two columns with voltages for position (column 2)and force (column 1). Conversion to position in mm is by the equation 15.66-position_voltage*4.2. Conversion to force in Newtons is by force_voltage*100*261*1.71*(-1/1000000). Data for tensile tests on PLMA, whole mouse bladder, and soft PDMS as measured on the version 1 tensile tester. Area is estimated from the included images with reference on the metal grips with a width of 4.4 mm and thickness of 0.3 mm.
PLMA样品的拉伸测试数据(采用V1型拉伸试验机测得)。数据包含两列电压数据,分别对应位移(第2列)与力(第1列)。位移(单位:毫米)可通过公式15.66 - 位移电压 × 4.2换算得到;力(单位:牛顿)可通过公式:力电压 × 100 × 261 × 1.71 × (-1/1000000)换算得到。PLMA、完整小鼠膀胱以及软质聚二甲基硅氧烷(PDMS)的拉伸测试数据,同样采用V1型拉伸试验机测得。试样截面积通过附带图像结合金属夹具进行估算,该金属夹具宽度为4.4 mm,厚度为0.3 mm。