Uniaxial creep test data for 13 CrMo 4 4 se material at 530 °C and a stress of 90.23 MPa
收藏资源简介:
The aim of the project was to compare various techniques for the assessment of remaining life for power plant components. In this context, creep tests were performed on three grades of low Cr steel, namely 1Cr0.5Mo (DIN 13CrMo 4 4), 0.5Cr0.5Mo0.25V (DIN 14MoV 6 3), and 2.25Cr1Mo (DIN 10CrMo 9 10). The creep tests were designed to provide a series of test pieces with defined creep strains ranging from 0.2 to 5 % for creep damage assessment. In addition, basic rupture data were determined for the steels in the new and service exposed conditions. Several creep laboratories participated in the test programme. At FZ Jülich the materials tested were new and service exposed 1Cr0.5Mo, new 0.5Cr0.5Mo0.25V and new 2.25Cr1Mo steels. The 1Cr0.5Mo service exposed specimens were taken from a pipe that had been in service at 525 oC for 250 000 h at 110 bar, and the 0.5Cr0.5Mo0.25V from a forging after 116 000 h service exposure at 530 °C, 176 bar. The creep data set contains test results determined at 530, 550, 600 and 625 °C and the longest test times were 26000 h for 1Cr0.5Mo service exposed, 14000 h for 1Cr0.5Mo new and 24000 h for new 0.5Cr0.5Mo0.25V.
本项目旨在对比评估电厂部件剩余寿命的各类技术手段。在此背景下,研究团队针对三种牌号的低铬钢开展了蠕变试验,分别为1Cr0.5Mo(DIN 13CrMo 4 4)、0.5Cr0.5Mo0.25V(DIN 14MoV 6 3)以及2.25Cr1Mo(DIN 10CrMo 9 10)。本次蠕变试验旨在制备一系列蠕变应变范围为0.2%至5%的试验试样,用于蠕变损伤评估。此外,研究人员还测定了新态与服役后态钢材的基础蠕变断裂数据。多家蠕变试验室参与了本试验项目。在德国于利希研究中心(FZ Jülich),本次试验涉及的材料包括新态与服役后态1Cr0.5Mo钢、新态0.5Cr0.5Mo0.25V钢以及新态2.25Cr1Mo钢。其中,服役后态1Cr0.5Mo钢试样取自一根在525℃、110bar工况下服役250000小时的管道;服役后态0.5Cr0.5Mo0.25V钢试样则取自一个在530℃、176bar工况下服役116000小时的锻件。本蠕变数据集涵盖了530℃、550℃、600℃及625℃下的试验结果,最长试验时长分别为:服役后态1Cr0.5Mo钢26000小时、新态1Cr0.5Mo钢14000小时、新态0.5Cr0.5Mo0.25V钢24000小时。