Uniaxial creep test data for X10CrMoVNb9 1 / X20CrMoV12 1 - dj material at 650 °C and a stress of 22 MPa
收藏官方服务:
资源简介:
Data generated in the scope of a project to investigate the influence of weld strength reduction on long-term integrity of power plant components made from heat-resistant martensitic steels.
本数据集源自一项研究项目,该项目旨在探究焊接强度降低对采用耐热马氏体钢(heat-resistant martensitic steels)制造的电厂部件长期完整性的影响。
创建时间:
2016-09-09