Uniaxial creep test data for 13 CrMo 4 4 se material at 530 °C and a stress of 99.86 MPa
收藏资源简介:
The aim of the project was to compare various techniques for the assessment of remaining life for power plant components. In this context, creep tests were performed on three grades of low Cr steel, namely 1Cr0.5Mo (DIN 13CrMo 4 4), 0.5Cr0.5Mo0.25V (DIN 14MoV 6 3), and 2.25Cr1Mo (DIN 10CrMo 9 10). The creep tests were designed to provide a series of test pieces with defined creep strains ranging from 0.2 to 5 % for creep damage assessment. In addition, basic rupture data were determined for the steels in the new and service exposed conditions. Several creep laboratories participated in the test programme. At FZ Jülich the materials tested were new and service exposed 1Cr0.5Mo, new 0.5Cr0.5Mo0.25V and new 2.25Cr1Mo steels. The 1Cr0.5Mo service exposed specimens were taken from a pipe that had been in service at 525 oC for 250 000 h at 110 bar, and the 0.5Cr0.5Mo0.25V from a forging after 116 000 h service exposure at 530 °C, 176 bar. The creep data set contains test results determined at 530, 550, 600 and 625 °C and the longest test times were 26000 h for 1Cr0.5Mo service exposed, 14000 h for 1Cr0.5Mo new and 24000 h for new 0.5Cr0.5Mo0.25V.
本项目旨在对比评估电站部件剩余寿命(remaining life)的各类技术。在此背景下,针对三种低铬钢牌号开展了蠕变试验(creep test),分别为1Cr0.5Mo(DIN 13CrMo 4 4)、0.5Cr0.5Mo0.25V(DIN 14MoV 6 3)以及2.25Cr1Mo(DIN 10CrMo 9 10)。本次蠕变试验旨在制备一批蠕变应变(creep strain)范围明确(0.2%至5%)的试样,用于蠕变损伤(creep damage)评估。此外,还针对上述钢材的全新及服役后状态,测定了基础蠕变断裂(rupture)数据。多家蠕变试验室参与了本次试验计划。在FZ Jülich(于利希研究中心)开展的试验中,受试材料涵盖全新及服役后的1Cr0.5Mo钢、全新0.5Cr0.5Mo0.25V钢与全新2.25Cr1Mo钢。其中,1Cr0.5Mo钢的服役试样取自一台在525℃、110巴(bar)工况下服役250000小时的管道;0.5Cr0.5Mo0.25V钢的服役试样则取自一件在530℃、176巴(bar)工况下服役116000小时的锻件。本蠕变数据集包含在530℃、550℃、600℃及625℃下测得的试验结果,最长试验时长分别为:服役态1Cr0.5Mo钢26000小时、全新1Cr0.5Mo钢14000小时,以及全新0.5Cr0.5Mo0.25V钢24000小时。