Small punch creep test data for P91 material at 600 °C and a load of 245 N

收藏
DataCite Commons2020-10-05 更新2025-05-18 收录
官方服务:

资源简介:

Data produced during work to evaluate the creep and fracture properties of P91 steel by small punch testing. The tests were performed on material extracted from the same pipe used in the INTEGRITY FP5 Growth Project (GRD 1/10886. 2005.), the data for which are also hosted at the JRC Petten ODIN portal.

本数据集源自通过小冲杆试验(small punch testing)评估P91钢蠕变与断裂性能的相关研究工作。试验所用材料取自INTEGRITY FP5增长项目(GRD 1/10886. 2005.)中使用的同一管材,该项目的相关数据同样托管于欧盟联合研究中心(Joint Research Centre,JRC)佩滕分中心的ODIN门户。