Uniaxial creep test data for AISI 316L ar material at 650 °C and a stress of 150 MPa (specimen identifier GC-01)
收藏官方服务:
资源简介:
Data created at JRC, Netherlands during the Horizon 2020 NUCOBAM project aiming to develop the qualification process and evaluate the in-service behaviour of AM materials, allowing the use of additively manufactured components in nuclear installations. The project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 945313.
本数据集由荷兰欧洲联合研究中心(JRC)于欧盟地平线2020(Horizon 2020)框架下的NUCOBAM项目中创建。该项目旨在开发增材制造(Additive Manufacturing,AM)材料的合格评定流程,并评估其服役行为,以实现增材制造构件在核设施中的应用。本项目已获得2014-2018年欧洲原子能共同体(Euratom)研究与培训计划下编号为945313的资助协议支持。
创建时间:
2024-10-15