Uniaxial creep test data for ER 316L sa wm material at 500 °C and a stress of 274 MPa (specimen identifier 35619)

收藏
DataCite Commons2023-08-30 更新2025-04-16 收录
官方服务:

资源简介:

Data created by ENEA, Italy during the Horizon 2020 GEMMA project on GenIV materials maturity, including test results from an SSRT round-robin on EUROTRANS/DEMETRA T91 in Pb at 400°C. This project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 755269.

本数据集由意大利ENEA在“地平线2020”计划(Horizon 2020)下的GEMMA项目中创建,该项目围绕第四代核反应堆材料成熟度(GenIV)展开研究,包含了400℃铅(Pb)环境中针对EUROTRANS/DEMETRA T91钢开展的慢应变速率拉伸试验(Slow Strain Rate Testing,SSRT)循环比对试验的测试结果。本项目获2014-2018年欧洲原子能共同体研究与培训计划(Euratom)资助,资助协议编号为755269。