Mechanical characterization and strain-rate sensitivity measurement by nanoindentation and crystal plasticity finite element modeling: Application to Ti-7Mo-3Nb-3Cr-3Al near β titanium alloy
收藏Mendeley Data2018-01-17 更新2026-04-09 收录
下载链接:
https://data.mendeley.com/datasets/ddxtvjjfdk/2
下载链接
链接失效反馈官方服务:
资源简介:
the supporting data for paper entitled 'Mechanical characterization and strain-rate sensitivity measurement by nanoindentation and crystal plasticity finite element modeling: Application to Ti-7Mo-3Nb-3Cr-3Al near β titanium alloy'
本数据集为题为《通过纳米压痕(nanoindentation)与晶体塑性有限元建模(crystal plasticity finite element modeling)开展力学表征及应变率敏感性测试:在Ti-7Mo-3Nb-3Cr-3Al近β型钛合金(near β titanium alloy)中的应用》的学术论文的配套支撑数据