遇见数据集

Dataset for Robust surface functionalization of PDMS through atmospheric pressure atomic layer deposition

收藏
DataCite Commons2024-06-04 更新2024-07-03 收录
官方服务:

资源简介:

The dataset is a basis for a publication of Robust surface functionalization of PDMS through atmospheric pressure atomic layer deposition, intended to be of chapter 3 in the corresponding dissertation. In this dataset, the research objective "Evaluating the use of atmospheric pressure atomic layer deposition (AP-ALD) in functionalizing the surface of polydimethylsiloxane flat substrates" was addressed. The data were collected using various characterization techniques (advanced microscopy, advanced spectroscopy, and newly developed barrier property testing). The presented data were in the form of images (jpg.) and origin file containing the XPS and barrier property data (opju).

提供机构:
4TU.ResearchData
创建时间:
2024-06-04
二维码
社区交流群
二维码
科研交流群
商业服务