Small punch creep test data for P91 material at 600 °C and a load of 314 N (third repeat test)

收藏
DataCite Commons2026-03-10 更新2026-05-04 收录
官方服务:

资源简介:

Data produced during work to evaluate the creep and fracture properties of P91 steel by small punch testing. The tests were performed on material extracted from the same pipe used in the INTEGRITY FP5 Growth Project (GRD 1/10886. 2005.), the data for which are also hosted at the JRC Petten ODIN portal.