Nanocrystalline thin films with 800 nm thickness were prepared by sol–gel method. To examine the influence of the annealing temperature on as-prepared films crystallization, the coatings were heated at temperature from 500 °C up to 600 °C for 20h. Structure of manufactured thin films was investigated using X-ray diffraction (XRD). The most visible lithium titanate phase was obtained after 20 h annealing at 550 °C.