This is the dataset that contains underlying data enabling to reproduce the findings reported in the paper: "Some notes about simulating nanoindentation with imperfect Berkovich tip". Data stored in folders starting with "Fig" contain data enabling to reporoduce the figures. In the case of "Fig1" folder, this is the Wolfram Mathematica notebook enabling to draw the plot of analytical functions presented in Fig. 1. "Fig2" folder contains the nodes and elements of the finite element meshes used. For the other figures, data contain the tabular data enabling to draw curves and surfaces presented in Figures 3-9. In addtion, contact element codes for the frictionless and Coulomb friction cases are stored in spearate folders.
创建时间:
2025-04-09